Polytetrafluoroethylene is the lowest-loss laminate in common use, and the most awkward to build with. Both facts matter when you decide how much of the stack-up should be PTFE.

PTFE laminate sheet prepared for machining

Overview

The lowest loss available, and the reason it is not used everywhere.

PTFE-based laminates such as RT/duroid 5880 sit at Dk 2.20 and Df 0.0009 measured at 10 GHz — roughly a third of the loss of a standard FR-4 and well below the Rogers 4000 series. For a millimetre-wave front end or a long low-loss run, that difference is the budget. Nothing else in the catalogue matches it.

The cost is mechanical. PTFE is soft, it moves under drill and press, and it does not bond to FR-4 prepreg without the right surface treatment. Layer count drops accordingly: an all-PTFE stack runs 2–8 layers, while a hybrid that puts PTFE only on the RF layers reaches 8–12. The engineering question is rarely whether PTFE works — it is how little of the board actually needs it.

Working Limits

What PTFE changes about the build.

Electrical

Parameter Value Why it matters
Dk (RT/duroid 5880) 2.20 at 10 GHz Wider traces for the same impedance, and less sensitivity to etch tolerance
Df (RT/duroid 5880) 0.0009 at 10 GHz The lowest loss figure we quote on any laminate
Hybrid with FR-4 PTFE signal layers, FR-4 core Keeps the RF layers on PTFE and the rest on the cheaper material

Mechanical

Parameter Value Why it matters
All-PTFE layer count 2–8 layers Soft substrate moves under press; bond and drill quality fall away above this
PTFE plus FR-4 hybrid 8–12 layers The practical route to a tall stack-up that still carries an RF layer
Surface finish Not recommended for HASL Solder levelling is too hot and too mechanically aggressive for the substrate

Dk and Df are quoted at 10 GHz because PTFE figures move with frequency and a value without its basis is not a specification. Every build runs to IPC Class 2 standard, Class 3 on request.

How Much PTFE

Four questions that size the PTFE content.

01

Is the loss budget actually binding?
Below 10 GHz, a Rogers 4350B usually clears the budget at lower cost and far less process risk.

02

Which layers carry the microwave?
Only those need PTFE. Everything else can stay FR-4 in a hybrid stack-up.

03

How many layers in total?
Past eight, an all-PTFE build is off the table and the hybrid becomes the only route.

04

Does anything need to bend?
PTFE is not a flex material. If the board flexes, the conversation moves to polyimide.

Process Notes

Three things that decide whether the build holds.

01

Bonding needs preparation

PTFE will not laminate to FR-4 prepreg as it arrives. The surface is treated before lay-up, and the press cycle is set for the two materials expanding differently rather than for an average of the two.

02

Drilling is a separate programme

The substrate is soft and abrasive filler is absent, so drill parameters are qualified on the actual laminate instead of inherited from the FR-4 programme. A drill recipe that works on FR-4 will smear here.

03

Ordered, not stocked

PTFE composites are ordered against confirmed demand, unlike standard FR-4 and the Rogers 4003C/4350B grades we keep on the shelf. Lead time is quoted per grade at the point of order.

Working out how little PTFE the design needs?

Send the frequency plan and the layer count. The answer names which layers go PTFE and which stay FR-4.

Get a Quote
WhatsApp

FAQ

PTFE questions that come up before quoting.

Do I need PTFE or is Rogers 4350B enough?

Below about 10 GHz, 4350B usually clears the loss budget at Dk 3.66 and Df 0.0037, and it processes much like FR-4. PTFE at Dk 2.20 and Df 0.0009 becomes the answer when the run length, the frequency or the antenna efficiency leaves no room in the budget.

Why does an all-PTFE stack stop at eight layers?

The substrate is soft and moves under press, so registration and bond quality degrade with each lamination cycle. Eight layers is the practical ceiling we will quote for an all-PTFE build; beyond that the hybrid route is the one that holds.

Can PTFE and FR-4 share one stack-up?

Yes, and it is the standard way to keep a millimetre-wave board affordable — PTFE on the layers that carry the RF, FR-4 on the rest, up to 8–12 layers. The two expand at different rates, so the press cycle is built around that difference.

Why is HASL not recommended?

Solder levelling puts the panel through a thermal and mechanical shock the substrate handles badly, and the finish itself is not what an RF surface needs. ENIG, immersion silver or immersion tin are the finishes specified on PTFE work.

Is PTFE available from stock?

No. PTFE composites are ordered against confirmed demand, with lead time quoted per grade. Standard FR-4, High-TG FR-4, Rogers 4003C/4350B and aluminium core are the grades held for quick-turn.

Want the PTFE content sized before layout?

Send the frequency plan and the stack-up. Quote in 24 hours, with the hybrid option priced alongside.

Get a Quote