Any-layer microvias, 0.1 mm laser drills and up to four lamination cycles — with the engineering review finished before the first panel is imaged, not after.

Any-layer HDI PCB with laser-drilled microvias

Overview

Density is a stack-up decision.

HDI PCB replaces part of the mechanical drill programme with laser-drilled microvias, finer conductors and sequential lamination. The payoff is routing density per square centimetre, shorter return paths and a workable escape for fine-pitch BGA — the combination that dense AI, RF and handheld hardware cannot be built without.

Many fabricators sell HDI as a feature list and hand the hard decisions back to the customer. We take the opposite position: an HDI stack-up is a set of coupled choices — via type, aspect ratio, lamination count, fill, impedance — and an error in any one of them surfaces only after lamination, when nothing can be reworked.

So the review happens before tooling. 80 CAM engineers work through more than 6,000 designs a month, confirming any-layer and stacked-via feasibility and returning engineering queries inside 24 hours. Fine-line imaging, 0.1 mm laser drilling, ±50 µm layer registration and 100% electrical test then carry the approved stack-up through to shipment.

Key Processes

Four points where an HDI build is won or lost.

01

Laser Drill Geometry

Microvia quality is set by pulse energy, copper surface and dielectric, not by one recipe reused on every panel. The drill programme is qualified on your actual laminate and copper weight, so a 0.1 mm via lands centred on its target pad instead of skimming the edge.

02

Via Stacking and Cycle Count

Stacking a via onto the one below multiplies density, but each additional press carries its own registration budget. Cycle count is modelled against your escape requirement before the quote, keeping any-layer work inside four lamination cycles and the build inside the layer count the design truly needs.

03

Via Fill and Planarity

Via-in-pad only survives assembly if the filled via is flat under a fine-pitch BGA. Filling, planarising and copper capping run as one controlled operation, and the surface is measured after plating rather than assumed — which keeps paste release and joint volume predictable lot to lot.

04

Microvia Integrity and Impedance

A microvia is a mechanical feature as much as an electrical one, and barrel integrity after thermal stress decides field life. Thermal screening runs alongside TDR coupon measurement — ±5% standard, ±3% on request — so electrical and mechanical confidence are proven from the same lot.

Process Capability

The build window, in numbers.

Parameter Capability
Laser microvia 0.1 mm minimum; stacked, staggered and any-layer constructions
Layer count 2–32 layers standard; 50+ on inquiry with sequential lamination
Lamination cycles Up to 4 for any-layer HDI; higher counts reviewed at engineering query
Min trace / space 0.075 mm / 0.075 mm
Board thickness 0.4–6.0 mm
Drill and aspect ratio Mechanical from 0.15 mm; 12:1 standard, 20:1 on inquiry
Impedance control ±5% standard, ±3% on request; TDR coupon per lot, data ships with CoC
Electrical test 100% — flying probe on prototypes, fixture on volume

UL 94 V-0 · IPC-6012 / IPC-A-600 · IPC Class 2 standard, Class 3 on request · Full matrix: see Capabilities.

Materials & Surface Finish

Laminate chosen for the via and the signal.

Standard FR-4Tg 130–150°C · the workhorse below 3 GHz
High-Tg FR-4Tg 170–180°C · holds through repeated reflow
Low-loss / high-speedMEGTRON-class laminates for fast edges
Rogers hybrid4003C / 4350B / 5880 · see Rogers PCB

ENIG (default; Au 3–6 µin over Ni 120–240 µin) · HASL-LF · OSP · Immersion Silver · Immersion Tin · Hard Gold (on request)

Not sure your microvia stack is buildable?

Send the stack-up — an engineer checks via type and cycle count before you commit.

Get a Quote
WhatsApp

Typical Applications

Where HDI density pays for itself.

16-layer any-layer HDI server board for AI accelerator cards

AI Accelerator Cards

16-layer any-layer server boards carrying accelerator and switch ASICs.

Impedance-controlled high-speed board for aerospace communications

Aerospace Communications

Dense impedance-controlled RF and datalink boards for airborne terminals.

High-density rigid-flex assembly for medical imaging electronics

Medical Imaging

High-channel-count imaging modules where board area is the hard constraint.

Low-loss Rogers board for a 5G massive-MIMO radio unit

5G Base Stations

Low-loss mixed-material boards for massive-MIMO radio units.

Related Articles

Engineering reading for dense designs.

FAQ

What engineers ask before an HDI order.

What is the smallest microvia you drill?

Laser microvias down to 0.1 mm; mechanical holes from 0.15 mm. Your practical minimum also depends on dielectric thickness and target pad size, which the CAM review confirms before tooling.

How many lamination cycles can my layer count take?

Any-layer builds are planned inside four cycles, with registration budgeted for every press. If the routing needs more, we test whether a staggered arrangement or a different layer count solves the same escape with fewer laminations.

How do you verify impedance on an HDI board?

TDR coupons run with every production panel: ±5% standard, ±3% on request. The measured data travels with the CoC, and a lot outside the window is held for engineering disposition rather than shipped.

Which files should I send for an HDI quote?

Gerber RS-274X or ODB++, drill and via files, plus a stack-up drawing if one exists. If the via strategy is still open, tell us the escape pitch and we will propose one.

What lead time applies to HDI builds?

Lead time is confirmed at quotation for the specific stack-up and cycle count, with expedited options available. If the schedule moves, we tell you when we know — not on the ship date.